Effect of moist vs. dry bonding to normal vs. caries-affected dentin with scotchbond multi-purpose plus

M. Nakajima, H. Sano, L. Zheng, J. Tagami, D. H. Pashley

Research output: Contribution to journalArticle

79 Citations (Scopus)

Abstract

Recent research in dentin bonding demonstrated the superiority of moist bonding over dry bonding on normal dentin, but it is unclear if this technique is also superior in bonding to caries-affected dentin. The purpose of this study was to evaluate the SEM appearance and bond strength of Scotchbond Multi-Purpose Plus (SMPP) to normal vs. caries-affected dentin bonded under moist vs. dry conditions, with and without polyalkenoic acid in the primer. Extracted carious human third molars were ground down by means of 600-grit SiC paper until the carious dentin no longer stained with caries detector solution. The flat surfaces were then primed, bonded, and built up with resin composite. After soaking in water for 1 day, the teeth were serially sectioned vertically into 5 or 6 slabs 0.7 mm thick. The bonded caries-affected areas were isolated by means of an ultrafine diamond bur to create an hourglass configuration with a cross-sectional area of 0.9 mm2. Bonded normal dentin was isolated the same way. Each specimen was attached to a Bencor device and tested in tension to failure. SMPP bonds to dry, normal dentin were only half as strong (21 ± 10 MPa, x̄ ± SD) as those made to moist, normal dentin (42 ± 9 MPa, p < 0.01). There was no significant difference between bonds made to normal vs. caries-affected dentin by means of the moist technique (42 ± 9 vs. 48 ± 4 MPa, respectively). Removal of the polyalkenoic acid from the primer lowered (p < 0.05) the bond strength of SMPP to cariesaffected dentin (38 ± 8 MPa). The benefits of moist bonding extend to caries-affected dentin. The polyalkenoic acid in the SMPP primer contributes to the high bond strength that can be achieved to caries-affected dentin.

Original languageEnglish (US)
Pages (from-to)1298-1303
Number of pages6
JournalJournal of Dental Research
Volume78
Issue number7
DOIs
StatePublished - Jan 1 1999

Fingerprint

Dentin
Acids
Scotchbond Multi-Purpose Plus
Diamond
Third Molar
Composite Resins
Dental Caries
Tooth
Equipment and Supplies

Keywords

  • Carious dentin
  • Dentin bonding
  • Resin adhesion

ASJC Scopus subject areas

  • Dentistry(all)

Cite this

Effect of moist vs. dry bonding to normal vs. caries-affected dentin with scotchbond multi-purpose plus. / Nakajima, M.; Sano, H.; Zheng, L.; Tagami, J.; Pashley, D. H.

In: Journal of Dental Research, Vol. 78, No. 7, 01.01.1999, p. 1298-1303.

Research output: Contribution to journalArticle

Nakajima, M. ; Sano, H. ; Zheng, L. ; Tagami, J. ; Pashley, D. H. / Effect of moist vs. dry bonding to normal vs. caries-affected dentin with scotchbond multi-purpose plus. In: Journal of Dental Research. 1999 ; Vol. 78, No. 7. pp. 1298-1303.
@article{107020b8cec0495594c7907f52ba1023,
title = "Effect of moist vs. dry bonding to normal vs. caries-affected dentin with scotchbond multi-purpose plus",
abstract = "Recent research in dentin bonding demonstrated the superiority of moist bonding over dry bonding on normal dentin, but it is unclear if this technique is also superior in bonding to caries-affected dentin. The purpose of this study was to evaluate the SEM appearance and bond strength of Scotchbond Multi-Purpose Plus (SMPP) to normal vs. caries-affected dentin bonded under moist vs. dry conditions, with and without polyalkenoic acid in the primer. Extracted carious human third molars were ground down by means of 600-grit SiC paper until the carious dentin no longer stained with caries detector solution. The flat surfaces were then primed, bonded, and built up with resin composite. After soaking in water for 1 day, the teeth were serially sectioned vertically into 5 or 6 slabs 0.7 mm thick. The bonded caries-affected areas were isolated by means of an ultrafine diamond bur to create an hourglass configuration with a cross-sectional area of 0.9 mm2. Bonded normal dentin was isolated the same way. Each specimen was attached to a Bencor device and tested in tension to failure. SMPP bonds to dry, normal dentin were only half as strong (21 ± 10 MPa, x̄ ± SD) as those made to moist, normal dentin (42 ± 9 MPa, p < 0.01). There was no significant difference between bonds made to normal vs. caries-affected dentin by means of the moist technique (42 ± 9 vs. 48 ± 4 MPa, respectively). Removal of the polyalkenoic acid from the primer lowered (p < 0.05) the bond strength of SMPP to cariesaffected dentin (38 ± 8 MPa). The benefits of moist bonding extend to caries-affected dentin. The polyalkenoic acid in the SMPP primer contributes to the high bond strength that can be achieved to caries-affected dentin.",
keywords = "Carious dentin, Dentin bonding, Resin adhesion",
author = "M. Nakajima and H. Sano and L. Zheng and J. Tagami and Pashley, {D. H.}",
year = "1999",
month = "1",
day = "1",
doi = "10.1177/00220345990780070301",
language = "English (US)",
volume = "78",
pages = "1298--1303",
journal = "Journal of Dental Research",
issn = "0022-0345",
publisher = "SAGE Publications Inc.",
number = "7",

}

TY - JOUR

T1 - Effect of moist vs. dry bonding to normal vs. caries-affected dentin with scotchbond multi-purpose plus

AU - Nakajima, M.

AU - Sano, H.

AU - Zheng, L.

AU - Tagami, J.

AU - Pashley, D. H.

PY - 1999/1/1

Y1 - 1999/1/1

N2 - Recent research in dentin bonding demonstrated the superiority of moist bonding over dry bonding on normal dentin, but it is unclear if this technique is also superior in bonding to caries-affected dentin. The purpose of this study was to evaluate the SEM appearance and bond strength of Scotchbond Multi-Purpose Plus (SMPP) to normal vs. caries-affected dentin bonded under moist vs. dry conditions, with and without polyalkenoic acid in the primer. Extracted carious human third molars were ground down by means of 600-grit SiC paper until the carious dentin no longer stained with caries detector solution. The flat surfaces were then primed, bonded, and built up with resin composite. After soaking in water for 1 day, the teeth were serially sectioned vertically into 5 or 6 slabs 0.7 mm thick. The bonded caries-affected areas were isolated by means of an ultrafine diamond bur to create an hourglass configuration with a cross-sectional area of 0.9 mm2. Bonded normal dentin was isolated the same way. Each specimen was attached to a Bencor device and tested in tension to failure. SMPP bonds to dry, normal dentin were only half as strong (21 ± 10 MPa, x̄ ± SD) as those made to moist, normal dentin (42 ± 9 MPa, p < 0.01). There was no significant difference between bonds made to normal vs. caries-affected dentin by means of the moist technique (42 ± 9 vs. 48 ± 4 MPa, respectively). Removal of the polyalkenoic acid from the primer lowered (p < 0.05) the bond strength of SMPP to cariesaffected dentin (38 ± 8 MPa). The benefits of moist bonding extend to caries-affected dentin. The polyalkenoic acid in the SMPP primer contributes to the high bond strength that can be achieved to caries-affected dentin.

AB - Recent research in dentin bonding demonstrated the superiority of moist bonding over dry bonding on normal dentin, but it is unclear if this technique is also superior in bonding to caries-affected dentin. The purpose of this study was to evaluate the SEM appearance and bond strength of Scotchbond Multi-Purpose Plus (SMPP) to normal vs. caries-affected dentin bonded under moist vs. dry conditions, with and without polyalkenoic acid in the primer. Extracted carious human third molars were ground down by means of 600-grit SiC paper until the carious dentin no longer stained with caries detector solution. The flat surfaces were then primed, bonded, and built up with resin composite. After soaking in water for 1 day, the teeth were serially sectioned vertically into 5 or 6 slabs 0.7 mm thick. The bonded caries-affected areas were isolated by means of an ultrafine diamond bur to create an hourglass configuration with a cross-sectional area of 0.9 mm2. Bonded normal dentin was isolated the same way. Each specimen was attached to a Bencor device and tested in tension to failure. SMPP bonds to dry, normal dentin were only half as strong (21 ± 10 MPa, x̄ ± SD) as those made to moist, normal dentin (42 ± 9 MPa, p < 0.01). There was no significant difference between bonds made to normal vs. caries-affected dentin by means of the moist technique (42 ± 9 vs. 48 ± 4 MPa, respectively). Removal of the polyalkenoic acid from the primer lowered (p < 0.05) the bond strength of SMPP to cariesaffected dentin (38 ± 8 MPa). The benefits of moist bonding extend to caries-affected dentin. The polyalkenoic acid in the SMPP primer contributes to the high bond strength that can be achieved to caries-affected dentin.

KW - Carious dentin

KW - Dentin bonding

KW - Resin adhesion

UR - http://www.scopus.com/inward/record.url?scp=0033278122&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0033278122&partnerID=8YFLogxK

U2 - 10.1177/00220345990780070301

DO - 10.1177/00220345990780070301

M3 - Article

C2 - 10403456

AN - SCOPUS:0033278122

VL - 78

SP - 1298

EP - 1303

JO - Journal of Dental Research

JF - Journal of Dental Research

SN - 0022-0345

IS - 7

ER -