Microtensile bond strengths of one-step self-etching adhesive systems

Ling Yu, Xiao yan Wang, Fucong Tian, Xue jun Gao

Research output: Contribution to journalArticle

2 Citations (Scopus)

Abstract

OBJECTIVE: To evaluate the microtensile bond strength of one-step self-etching adhesives to dentin in vitro. METHODS: Three commercially available one-step self-etching bonding systems (group A: Adper Prompt, group B: Clearfil S(3) Bond, group C: Xeno III) were compared with two-step self-etching adhesive (group D: Clearfil SE Bond) in this study. The microtensile bond strength was determined with microtensile tester and the fractured bonding surfaces were observed under stereomicroscope and scanning electronic microscope (SEM). The mean bond strengths were analyzed using one-way ANOVA test (P < 0.05). RESULTS: Mean microtensile bond strengths of group C, B, A and D were (34.59 +/- 3.46), (30.46 +/- 3.82), (23.36 +/- 2.55) and (45.06 +/- 5.29) MPa, respectively. Group D showed the highest bond strength (P < 0.01). CONCLUSIONS: Two-step self-etching adhesive had a higher bond strength than one-step self-etching adhesive systems, although all of them can satisfy the clinical requirements.

Original languageEnglish (US)
Pages (from-to)240-241
Number of pages2
JournalZhonghua kou qiang yi xue za zhi = Zhonghua kouqiang yixue zazhi = Chinese journal of stomatology
Volume42
Issue number4
StatePublished - Jan 1 2007
Externally publishedYes

Fingerprint

Adhesives
Dentin
Analysis of Variance

ASJC Scopus subject areas

  • Medicine(all)

Cite this

Microtensile bond strengths of one-step self-etching adhesive systems. / Yu, Ling; Wang, Xiao yan; Tian, Fucong; Gao, Xue jun.

In: Zhonghua kou qiang yi xue za zhi = Zhonghua kouqiang yixue zazhi = Chinese journal of stomatology, Vol. 42, No. 4, 01.01.2007, p. 240-241.

Research output: Contribution to journalArticle

@article{653ad827cd6c4c3c8e042d8cb7c083dc,
title = "Microtensile bond strengths of one-step self-etching adhesive systems",
abstract = "OBJECTIVE: To evaluate the microtensile bond strength of one-step self-etching adhesives to dentin in vitro. METHODS: Three commercially available one-step self-etching bonding systems (group A: Adper Prompt, group B: Clearfil S(3) Bond, group C: Xeno III) were compared with two-step self-etching adhesive (group D: Clearfil SE Bond) in this study. The microtensile bond strength was determined with microtensile tester and the fractured bonding surfaces were observed under stereomicroscope and scanning electronic microscope (SEM). The mean bond strengths were analyzed using one-way ANOVA test (P < 0.05). RESULTS: Mean microtensile bond strengths of group C, B, A and D were (34.59 +/- 3.46), (30.46 +/- 3.82), (23.36 +/- 2.55) and (45.06 +/- 5.29) MPa, respectively. Group D showed the highest bond strength (P < 0.01). CONCLUSIONS: Two-step self-etching adhesive had a higher bond strength than one-step self-etching adhesive systems, although all of them can satisfy the clinical requirements.",
author = "Ling Yu and Wang, {Xiao yan} and Fucong Tian and Gao, {Xue jun}",
year = "2007",
month = "1",
day = "1",
language = "English (US)",
volume = "42",
pages = "240--241",
journal = "Zhonghua kou qiang ke za zhi [Chinese journal of stomatology]",
issn = "1002-0098",
publisher = "Zhonghua Yixuehui Zazhishe",
number = "4",

}

TY - JOUR

T1 - Microtensile bond strengths of one-step self-etching adhesive systems

AU - Yu, Ling

AU - Wang, Xiao yan

AU - Tian, Fucong

AU - Gao, Xue jun

PY - 2007/1/1

Y1 - 2007/1/1

N2 - OBJECTIVE: To evaluate the microtensile bond strength of one-step self-etching adhesives to dentin in vitro. METHODS: Three commercially available one-step self-etching bonding systems (group A: Adper Prompt, group B: Clearfil S(3) Bond, group C: Xeno III) were compared with two-step self-etching adhesive (group D: Clearfil SE Bond) in this study. The microtensile bond strength was determined with microtensile tester and the fractured bonding surfaces were observed under stereomicroscope and scanning electronic microscope (SEM). The mean bond strengths were analyzed using one-way ANOVA test (P < 0.05). RESULTS: Mean microtensile bond strengths of group C, B, A and D were (34.59 +/- 3.46), (30.46 +/- 3.82), (23.36 +/- 2.55) and (45.06 +/- 5.29) MPa, respectively. Group D showed the highest bond strength (P < 0.01). CONCLUSIONS: Two-step self-etching adhesive had a higher bond strength than one-step self-etching adhesive systems, although all of them can satisfy the clinical requirements.

AB - OBJECTIVE: To evaluate the microtensile bond strength of one-step self-etching adhesives to dentin in vitro. METHODS: Three commercially available one-step self-etching bonding systems (group A: Adper Prompt, group B: Clearfil S(3) Bond, group C: Xeno III) were compared with two-step self-etching adhesive (group D: Clearfil SE Bond) in this study. The microtensile bond strength was determined with microtensile tester and the fractured bonding surfaces were observed under stereomicroscope and scanning electronic microscope (SEM). The mean bond strengths were analyzed using one-way ANOVA test (P < 0.05). RESULTS: Mean microtensile bond strengths of group C, B, A and D were (34.59 +/- 3.46), (30.46 +/- 3.82), (23.36 +/- 2.55) and (45.06 +/- 5.29) MPa, respectively. Group D showed the highest bond strength (P < 0.01). CONCLUSIONS: Two-step self-etching adhesive had a higher bond strength than one-step self-etching adhesive systems, although all of them can satisfy the clinical requirements.

UR - http://www.scopus.com/inward/record.url?scp=77954071068&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=77954071068&partnerID=8YFLogxK

M3 - Article

VL - 42

SP - 240

EP - 241

JO - Zhonghua kou qiang ke za zhi [Chinese journal of stomatology]

JF - Zhonghua kou qiang ke za zhi [Chinese journal of stomatology]

SN - 1002-0098

IS - 4

ER -